Today is Email Alert  RSS

Study on Applicability of Oil Casing Material 110Cr13S for Offshore Oil and Gas Fields

Expand
  • Zhanjiang Branch Company,CNOOC(China) Co.,Ltd.,Zhanjiang 524057,China

Received date: 2023-01-26

  Revised date: 2023-02-15

  Accepted date: 2023-03-16

  Online published: 2023-08-23

Abstract

 In order to evaluate the applicability of 110Cr13S oil casing steel in offshore oil and gas field development projects,the corrosion behavior of 110Cr13S steel in simulated high temperature,high pressure,CO2 and H2S coexisting corrosion environments under well of deep water oil and gas fields was studied using exposure corrosion tests,in-situ electrochemical tests,stress corrosion tests.Scanning electron microscopy,energy spectrometer,electrochemical workstation,slow strain rate tensile testing machine were used to study the corrosion morphology,corrosion product composition,electrochemical behavior and slow strain rate tensile curves of 110Cr13S oil casing steel under the conditions of 129.5 ℃,H2S partial pressure of 358 Pa and CO2 partial pressure of 2.754 MPa.Results showed that the average corrosion rate of 110Cr13S steel was 0.004 4 mm/a under the simulated deep sea oil and gas field well conditions,and a dense and complete passivation film was formed on the surface of the sample,which presented good corrosion resistance and excellent resistance to sulfide stress corrosion cracking.Therefore,110Cr13S oil casing steel was suitable for selecting oil casing materials for oil and gas well development under conditions of deep water,high temperature,high pressure,CO2 and H2S coexisting conditions.

Cite this article

JIANG Donglei, YU Yi, WANG Heng, DIAO Huan, XIAO Tan, WANG Yinghao . Study on Applicability of Oil Casing Material 110Cr13S for Offshore Oil and Gas Fields[J]. Materials Protection, 2023 , 56(7) : 105 -109 . DOI: 10.16577/j.issn.1001-1560.2023.0168

References

[1] YEVTUSHENKO O,BETTGE D,BOHRAUS S,et al.Corrosion behavior of steels for CO2 injection[J].Process Safety and Environmental Protection,2014,92(1): 108-118.

[2] ZHANG Z,ZHANG N,LIU Z,et al.Synergistic effects of corrosion time and stress on corrosion of casing steel in H2S/CO2 gas wells [J].Materials and Corrosion,2018,69(3):386-392.

[3] LIU Z,GAO X,LI J,et al.Corrosion behaviour of low-alloy martensite steel exposed to vapour-saturated CO2 and CO2-saturated brine conditions [J].Electrochimica Acta,2016,213: 842-855.

[4] 黄廷林,赵建伟,李仲恺,等.陇东油田采出水系统的腐蚀及防护[J].西安建筑科技大学学报: 自然科学版,2002,34(4): 320-324.HUANG T L,ZHAO J W,LI Z K,et al.Corrosion and protection of produced water system in Longdong Oilfield[J] Journal of Xi’an University of Architecture and Technology: Natural Science Edition,2002,34 (4): 320-324.

[5] WANG H W,CAI J Y,JEPSON W P.CO2 corrosion mechanistic modeling and prediction in horizontal slug flow:NACE International Corrosion Conference and Exposition[C].Denver: NACE,2022: 02238.

[6] LIU Z Y,WANG X Z,LIU R K,et al.Electrochemical and sulfide stress corrosion cracking behaviors of tubing steels in a H2 S/CO2 annular environment[J].Journal of Materials Engineering and Performance,2014,23(4):1 279-1 287.

[7] 万里平,孟英峰,李 皋,等.H2S/CO2共存聚合物钻井液中腐蚀产物膜分析[J].应用基础与工程科学学报,2012,20(5): 863-873.WAN L P,MENG Y F,LI G,et al.Analysis of corrosion product film in H2 S/CO2 coexisting polymer drilling fluid[J].Journal of Applied Basic and Engineering Sciences,2012,20 (5): 863-873.

[8] JIANG X,QU D,SONG X,et al.Critical water content for corrosion of X65 mild steel in gaseous,liquid and supercritical CO2 stream[J].International Journal of Greenhouse Gas Control,2019,85: 11-22.

[9] CHOI Y S,NESIC S,LING S.Effect of H2 S on the CO2 corrosion of carbon steel in acidic solutions[J].Electrochimica Acta,2011,56(4): 1 752-1 760.

[10] SUN W,NESIC S,PAPAVINASAM S.Kinetics of iron sulfide and mixed iron sulfide/carbonate scale precipitation in CO2/H2S corrosion: NACE International Corrosion Conference and Exposition [C].[S.l.]: NACE,2006.

[11] LI K,ZENG Y,LUO J L.Influence of H2S on the general corrosion and sulfide stress cracking of pipelines steels for supercritical CO2 transportation [J].Corrosion Science,2021,190: 109639.

[12] HU Y,GUO P,YAO Z,et al.Corrosion Behaviour of Drill Pipe Steel in CO2-H2S Environment[J].International Journal of Electrochemical Science,2017,12(7): 6 705-6 713.

[13] YIN Z F,LIU L,WANG Y,et al.Study on Iron Sulphide Inhibition and Corrosion of 80S and 110SS steels in Acid Solutions Containing H2S and CO2[J].International Journal of Electrochemical Science,2020,15: 10 825-10 843.

[14] 叶 帆,葛鹏莉,许艳艳,等.H2S/CO2环境中pH 值对腐蚀产物膜以及腐蚀速率的影响[J].材料保护,2020,53(7): 55-60.YE F,GE P L,XU Y Y,et al.Effect of pH on corrosion product film and corrosion rate in H2S/CO2 environment [J]Materials Protection,2020,53 (7): 55-60.

[15] CHENG X,SHI Z,GLASS N,et al.A review of PEM hydrogen fuel cell contamination: Impacts,mechanisms,and mitigation[J].Journal of Power Sources,2007,165(2):739-756.

[16] ZHOU C,FANG B,WANG J,et al.Effect of interaction between corrosion film and H2 S/CO2 partial pressure ratio on the hydrogen permeation in X80 pipeline steel[J].Corrosion Engineering,Science and Technology,2020,55(5):392-399.

[17] ZHAO X,HUANG W,LI G,et al.Effect of CO2/H2S and applied stress on corrosion behavior of 15Cr tubing in oil field environment[J].Metals,2020,10(3): 409.

[18] 任呈强.N80 油管钢在含CO2/H2S 高温高压两相介质中的电化学腐蚀行为及缓蚀机理研究[D].西安: 西北工业大学,2003.REN C Q.Study on electrochemical corrosion behavior and corrosion inhibition mechanism of N80 tubing steel in hightemperature and high-pressure two-phase medium containing CO2/H2S [D].Xi’an: Northwestern Polytechnical University,2003.

[19] 余 意,蒋东雷,刁 欢,等.海上油气田用TN110Cr13M材质油套管的腐蚀电化学行为[J].腐蚀与防护,2022,43(7):98-101.YU Y,JIANG D L,DIAO H,et al.Electrochemical Corrosion Behavior of TN110Cr13M Casing in Offshore Oil and Gas Fields[J].Corrosion & Protection,2022,43(7):98-101.
Outlines

/