Evaluation of the Application Effect and Improvement Method of Corrosion Monitoring Technology for Buried Thermal Insulation Pipelines

Expand
  • 1.School of Mechanical Engineering,Xi’an Traffic Engineering Institute,Xi’an 710300,China;2.Pengzhou Gas Field (Marine) Development Project Department,Sinopec Southwest Oil and Gas Branch,Chengdu 610000,China

Received date: 2023-02-26

  Revised date: 2023-03-12

  Accepted date: 2023-04-17

  Online published: 2023-08-25

Abstract

In order to further clarify the cathodic protection effect of buried thermal insulation pipeline,improve the cathodic protection monitoring technology,reduce oilfield maintenance costs and ensure the safe operation of buried insulation pipeline in oilfield,the detection and monitoring tests of a buried thermal insulation delivery pipeline were conducted,the field application effect of the detection and monitoring technology for buried thermal insulation delivery pipelines in oil fields at present was analyzed,and a stable and inexpensive external corrosion monitoring device was proposed for pipelines inside the insulation layer.Results showed that the accuracy of the test results of outer anti-corrosive coating would be affected by the protective layer,when using PCM,ACVG and DCVG technologies.Using a high-definition magnetic flux leakage detector to detect the corrosion status of pipelines,the detection result error was 6%,but the detection results could not distinguish whether there was metal loss on the inner or outer walls,and the excavation verification was required.Due to the current shielding effect of anti-corrosive insulation layer,the measurement value of cathodic protection potential could not characterize the true potential of the pipeline.The designed external corrosion monitoring device for buried thermal insulation pipelines based on metal potential difference could effectively monitor the water ingress of insulation layers of buried thermal insulation pipeline and the cathodic protection potential of pipelines for a long time.

Cite this article

XUE Kailin, HU Zhiqiang, LIU Lele . Evaluation of the Application Effect and Improvement Method of Corrosion Monitoring Technology for Buried Thermal Insulation Pipelines[J]. Materials Protection, 2023 , 56(8) : 201 -209 . DOI: 10.16577/j.issn.1001-1560.2023.0205

References

[1] 胡士信,董 旭.我国管道防腐层技术现状[J].油气储运,2004,23(7):4-8.HU S X,DONG X.The Technical Status Quo and Disparities in China’s Pipeline Coating Industry[J].Oil & Gas Storage and Transportation,2004,23(7): 4-8.

[2] 张文艳,侯 胜,熊 娟,等.硬质聚氨酯泡沫塑料保温层对埋地管道的影响及对策[J].石油和化工设备,2012,15(10):78-80.ZHANG W Y,HOU S,XIONG J,et al.Influence of rigid polyurethane foam insulation layer on buried pipelines and countermeasures[J].Petro & Chemical Equipment,2012,15(10):78-80.

[3] 常礼明,胡光兴,张宗前.PCM 技术在油气管道防腐层检测中的应用[J].中国石油和化工标准与质量,2017,37(21):46-47.CHANG L M,HU G X,ZHANG Z Q.Application of PCM Technology in Anticorrosion Coating Inspection of Oil and Gas Pipelines [J].China Petroleum and Chemical Standard and Quality,2017,37(21): 46-47.

[4] GB/T 19285-2014,埋地钢质管道腐蚀防护工程检验[S].GB/T 19285-2014,Inspection of corrosion protection for buried steel pipelines[S].

[5] GB/T 21246-2007,埋地钢质管道阴极保护参数测量方法[S].GB/T 21246-2007,Measurement method for cathodic protection parameters of buried steel pipelines[S].

[6] GB/T 50538-2010,埋地钢质管道防腐保温层技术标准[S].GB/T 50538-2010,Technical standard for anti-corrosion and insulation coatings of buried steel pipeline[S].

[7] 孙灵念,区进军.管道防腐层检测技术在油田生产中的应用[J].油气储运,2002,21(1):47-49.SUN L N,QU J J.The Application of Pipeline Coating Detection Technology In Oilfield Pipelines [J].Oil & Gas Storage and Transportation,2002,21(1): 47-49.

[8] 王永峰.管道防腐层的检查及分析技术探讨[J].全面腐蚀控制,2019,33(5):105-107.WANG Y F.Discussion on Inspection and Analysis Technology of Pipeline Anticorrosive Coating[J].Total Corrosion Control,2019,33(5): 105-107.

[9] 曹继丹.油田管道防腐层检测及管道维护探析[J].化学工程与装备,2019,267(4):169-182.CAO J D.Exploration of Anticorrosive Coating Inspection and Pipeline Maintenance for Oilfield Pipelines[J].Chemical Engineering & Equipment,2019,267(4):169-182.

[10] ZHAO Q Y,ZHOU J T,XIA Q W,et al.Non-Destructive Testing of Steel Corrosion Fluctuation Parameters Based on Spontaneous Magnetic Flux Leakage and Its Relationship with Steel Bar Diameter[J].Materials,2019,12(24): 4116.

[11] 魏如鹏.油田管道检测与修复技术的应用现状分析[J].化工管理,2019,538(31):120-133.WEI R P.Analysis of the Application Status of Oilfield Pipeline Inspection and Repair Technology[J].Chemical Engineering Management,2019,538(31):120-133.

[12] 杨洪波.埋地压力管道检测方法选择的相关分析[J].化工设计通讯,2018,44(1):38-69.YANG H B.Correlation Analysis of Detection Methods for Buried Pressure Pipeline[J].Chemical Engineering Design Communications,2018,44(1):38-69.

[13] 何 萍.埋地压力管道检测方法选择的探讨[J].化工设计通讯,2017,43(8):134-175.HE P.Discussion on Selection of Detection Method for Buried Pressure Pipeline [J].Chemical Engineering Design Communications,2017,43(8):134-175.

[14] GB/T 21448-2008,埋地钢质管道阴极保护技术规范[S].GB/T 21448-2008,Specification of cathodic protection for underground steel pipelines[S].

[15] 刘志军,杜全伟,王维斌,等.埋地保温管道阴极保护有效性影响因素及技术现状[J].油气储运,2015,34(6):576-579.LIU Z J,DU Q W,WANG W B,et al.Influence factors for effectiveness and current status of cathodic protection for buried insulated pipelines[J].Oil & Gas Storage and Transportation,2015,34(6): 576-579.

[16] BRENNA A,LAZZARI L,PEDEFERRI M P,et al.Monitoring cathodic protection of buried pipeline by means of a potential probe with an embedded zinc reference electrode[J].Materials & Design,2016,114(10):194-201.

[17] 刘远法,周 屹.基于Arduino 单片机的解魔方机器人——控制部分[J].电脑知识与技术,2016,12(7):171-173.LIU Y F,ZHOU Y.The Robot Can Restore A Rubik’s Cube Based on Arduino Microcontroller—The Control Module[J].Computer Knowledge and Technology,2016,12 (7):171-173.

[18] 宗培源.基于DS18B20 的多路温度采集报警系统设计[J].化学工程与装备,2019,274(11):250-251.ZONG P Y.Design of a multi-channel temperature acquisition and alarm system based on DS18B20 [J].Chemical Engineering & Equipment,2019,274(11):250-251.
Outlines

/